    Pengaruh Temperatur Austenisasi Terhadap Sifat Mekanis dan Struktur Mikro Paduan (FeCu)–1.5(AlCNT) Dengan Metode Metalurgi Serbuk

    Effect of Austenization Temperature on Mechanical Properties and Microstructure of (FeCu)-1.5(AlCNT) Alloy Using the Powder Metallurgy Methods

    Thumbnail
    View/Open
    Cover (4.966Mb)
    Fulltext (5.574Mb)
    Date
    2025
    Author
    Widodo, Mhd Arie
    Advisor(s)
    Suprianto
    Metadata
    Show full item record
    Abstract
    (FeCu)-(AlCNT) alloy made by powder metallurgy is a combined alloy in order to obtain good mechanical properties and can be further improved mechanical properties by heat treatment process. Hardening is a heat treatment process that aims to improve the mechanical properties of a material by heating and cooling in certain time intervals and cooling media. This study analyzes the effect of heat treatment temperature on (FeCu)-(AlCNT) alloy. Variations used are non heat treatment, 800°C, 850°C and 900°C with a holding time of 30 minutes and then cooled quickly using water cooling media. The test results showed that the highest density was obtained at 900°C heat treatment of 6.14 g/cm3, while the lowest density was obtained from the alloy without heat treatment process with a value of 5.42 g/cm3. The highest Vickers hardness obtained in the heat treatment with a temperature of 900°C with a value of 160.5 VHN, while the lowest Vickers hardness obtained from the alloy without heat treatment with a value of 91.8 VHN. Compressive testing get the highest yield stress value of 357.35 Mpa on heat treatment with a temperature of 900°C, while without heat treatment get the lowest yield stress value of 242.71 Mpa. The lowest wear rate obtained in the heat treatment with a temperature of 900°C amounted to 1.998 x 10-7 mm3/Nmm, while the highest wear rate obtained in the alloy without heat treatment amounted to 4.528 x 10-7 mm3/Nmm. The heat treatment process can improve the microstructure of the alloy which makes the grain boundaries look smoother which supports the reduction and size reduction of porosity in the (FeCu)-(AlCNT) alloy.
    URI
    https://repositori.usu.ac.id/handle/123456789/100661
    Collections
    • Undergraduate Theses [901]

    Repositori Institusi Universitas Sumatera Utara (RI-USU)
    Universitas Sumatera Utara | Perpustakaan | Resource Guide | Katalog Perpustakaan
    DSpace software copyright © 2002-2016  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    Atmire NV
     

     

    Browse

    All of USU-IRCommunities & CollectionsBy Issue DateTitlesAuthorsAdvisorsKeywordsTypesBy Submit DateThis CollectionBy Issue DateTitlesAuthorsAdvisorsKeywordsTypesBy Submit Date

    My Account

    LoginRegister

    Repositori Institusi Universitas Sumatera Utara (RI-USU)
    Universitas Sumatera Utara | Perpustakaan | Resource Guide | Katalog Perpustakaan
    DSpace software copyright © 2002-2016  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    Atmire NV