dc.description.abstractFabrication of composite magnet material based on Barium Heksaferit with the addition FeB and silicone rubber as filler has been successfully prepared. The raw materials Barium Heksaferit and FeB separately milled by using Planetary Ball Mill (PBM) for 24 hours and High Energy Milling (HEM) for 1 hour and then mixed by using PBM with composition ratio BaFe12O19: FeB are 97: 3, 95: 5, and 93: 7 %weight. The powder has mixed calcined at 900 °C, then added silicone rubber 20, 30, 40, and 50% weight as filler composite materials. The caracterization of materials are the microstructure (XRD), bulk density, magnetic properties (VSM), and the tensile test. The XRD results showed the addition of FeB increasing phases of hematite (Fe2O3). The results show the highest bulk density value in the addition of 20% weight of silicone rubber is 2.251 ×10- 3kg/m3 and coercivity value, jHC = 2,85× A/m and young modulus value is 0.99 MPa. The results were obtained permanent magnet composites are durable because has a high coercivity.en_US
dc.language.isoiden_US
dc.publisherUniversitas Sumatera Utaraen_US
dc.subjectComposite magneten_US
dc.subjectBarium Heksaferiten_US
dc.subjectferro boronen_US
dc.subjectsilicone rubberen_US
dc.subjectcharacterizationen_US
dc.titleKarakterisasi Magnet Komposit Barium Heksaferit dengan Penambahan Feb sebagai Matrik dan Silicone Rubber sebagai Filleren_US
dc.typeThesisen_US
dc.identifier.nimNIM120801073
dc.identifier.nidnNIDN0003055713
dc.identifier.kodeprodiKODEPRODI45201#Fisika
dc.description.pages72 Halamanen_US
dc.description.typeSkripsi Sarjanaen_US


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record