dc.description.abstractImproving the mechanical properties of resin modified glass ionomer cement (RMGIC) repair materials have been carried out, one of which is by adding nanohydroxyapatite. Nano-hydroxyapatite is a biomaterial of calcium phosphate compounds with a powder size of less than 100 nm which can be synthesized from natural materials, namely tilapia (Oreochromis niloticus) scales. Tilapia scales were synthesized by calcination process to obtain hydroxyapatite powder, size reduction using a ball mill machine to obtain nano-hydroxyapatite powder (51.71 nm). The aim of the study was to determine the difference in the surface hardness of RMGIC after adding 2%, 5% and 8% of nano-hydroxyapatite by weight of tilapia (Oreochromis niloticus) scales. The research method is a laboratory experiment with a post test only control group design. The research sample is in the form of tablets with a diameter of 5 mm and a height of 2 mm. There were four groups of research samples namely group 1 (without the addition of hydroxyapatite), group 2 (addition of nano-hydroxyapatite of 2%), group 3 (addition of nano-hydroxyapatite of 5%) and group 4 (addition of nanohydroxyapatite of 8%) respectively. Each group consists of 10 samples. The ratio of RMGIC powder:nano-hydroxyapatite:liquid for each group was 0.32:0.00:0.10g ; 0.31;0.01:0.10g ; 0.30;0.02;0.10g ; 0.29;0.03:0.10g. Stir until homogeneous then put into a mold with a diameter of 5 mm and a height of 2 mm which is coated with celluloid strips then put a 1 kg load, give it a light cured light for 20 seconds. Surface hardness test using Vickers Hardness Tester. The mean surface hardness results of RMGIC in groups 1,2,3,4 were 76.88 ± 1.97VHN; 76.71±3.68VHN; 52.69±3.85VHN; 45.96±5.80VHN. Data analysis using one way anova test showed that there was a significant difference in surface hardness of RMGIC (p≤0.05) after the addition of nano-hydroxyapatite. There was a decrease in the surface hardness of the SIKMR group with the addition of nano-hydroxyapatite.en_US
dc.language.isoiden_US
dc.publisherUniversitas Sumatera Utaraen_US
dc.subjectGlass Ionomer Cementen_US
dc.subjectnano-hydroxyapatiteen_US
dc.subjectTilapia (Oreochromis niloticus) SCALESen_US
dc.titleKekerasan Permukaan Semen Ionomer Kaca Modifikasi Resin setelah Penambahan 2, 5 dan 8% Berat Nano-Hidroksiapatit Sisik Ikan Nila (Oreochromis Niloticus)en_US
dc.typeThesisen_US
dc.identifier.nimNIM190600188
dc.identifier.nidnNIDN0011098205
dc.identifier.kodeprodiKODEPRODI12201#Pendidikan Dokter Gigi
dc.description.pages75 Halamanen_US
dc.description.typeSkripsi Sarjanaen_US


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record