dc.description.abstractTensile bond strength as one of the mechanical properties of resin modified glass ionomer cement needs to be considered in order to provide better adhesion with the tooth surface. Several studies state that adhesion strength can increase if hydroxyapatite is added. Hydroxyapatite can be synthesized from nature such as tilapia fish scales (Oreochromis niloticus) and can be broken down into nanoparticles. The aim of this research was to obtain the proportion and differences in fracture categories of resin modified glass ionomer cement without the addition of nanohydroxyapatite and with the addition of 5% by weight of nano-hydroxyapatite from tilapia fish scales (Oreochromis niloticus) on tooth enamel. This research used tabletshaped samples with a diameter of 4 mm and a height of 2 mm which had previously been tested for tensile adhesive strength with two test groups, namely group 1 (without the addition of nano-hydroxyapatite) and group 2 (addition of 5% by weight of nanohydroxyapatite). The sample size for each group is 10 samples. After the tensile adhesive strength test was carried out, the sample was soaked in distilled water solution to keep it moist. Then, the fracture was observed using a Stereomicroscope and Scanning Electron Microscope (SEM). The results of observations of restoration material fractures on the tooth enamel surface were categorized into cohesive, adhesive and mixed. Data were tested using the Chi-Square test (p<0.05). The results of the fracture analysis in group 1 are in the mixed failure category for 8 samples, cohesive failure for 1 sample, and adhesive failure for 1 sample. In group 2, namely mixed failure, 10 samples. It can be concluded that there is no significant difference in fracture between groups 1 and 2. The best fracture occurs in group 2 which is directly proportional to the previous tensile strength test value with a total of 10 mixed fracture categories.en_US
dc.language.isoiden_US
dc.publisherUniversitas Sumatera Utaraen_US
dc.subjectTensile bond strengthen_US
dc.subjectGlass Ionomeren_US
dc.subjectTilapia Scales (Oreochromis niloticus)en_US
dc.subjectEnamelen_US
dc.subjectSDGsen_US
dc.titleAnalisis Patahan Semen Ionomer Kaca Modifikasi Resin Setelah Penambahan 5% Berat Nano-Hidroksiapatit Sisik Ikan Nila (Oreochromis Niloticus) yang Direkatkan pada Email Gigien_US
dc.title.alternativeFailure Analysis of Resin Modified Glass Ionomer Cement after Addition 5% Weight of Tilapia Scales (Oreochromis niloticus) to Enamelen_US
dc.typeThesisen_US
dc.identifier.nimNIM200600031
dc.identifier.nidnNIDN0011098205
dc.identifier.kodeprodiKODEPRODI12201#Pendidikan Dokter Gigi
dc.description.pages62 Pagesen_US
dc.description.typeSkripsi Sarjanaen_US


Files in this item

Thumbnail
Thumbnail
Thumbnail
Thumbnail
Thumbnail

This item appears in the following Collection(s)

Show simple item record