dc.description.abstract | Plasticy Retention Index (PRI) is a measure of rubber's resistance to wear
and tear or oxidation at high temperatures. The PRI value was measured from the
comparison of the plasticity value of the rubber before being burnt (P0) and the
plasticity value of the rubber after being burnt for 30 minutes at 140°C (P30). The
Plasticity Retention Index (PRI) is a simple and short test carried out to measure
the resistance of elasticity to degradation due to oxidation at high temperatures or
wear and tear which is determined using the Wallace Plastimeter. The PRI test on
the SIR 20 Crumb Rubber sample was carried out using the Wallace Rapid
Plastimeter method. From the results of tests that have been carried out in the PT
Rubber Hock Lie Sunggal laboratory are 74 ; 72 ; 70 ; 76 and 71. Based on the
Regulation of the Minister of Trade no. 26 of 2021, one of which regulates the
application of SPPT SNI 1903: 2017 includes technical specifications for natural
rubber of Standard Indonesian Rubber (SIR), The Plasticity Retention Index (PRI)
value which greatly influences the quality of rubber because the greater the value
produced, the more resistant the rubber is to degradation. at high temperatures it
will get better. . The results of this test indicate that the sample has met the quality
requirements set by the government. A high PRI value indicates that rubber has a
molecular chain that is resistant to degradation by oxidation. Meanwhile, a low
PRI value indicates that rubber is easily oxidized to become soft rubber. | en_US |
dc.language.iso | id | en_US |
dc.publisher | Universitas Sumatera Utara | en_US |
dc.subject | Rubber's resistance | en_US |
dc.subject | Crumb Rubber | en_US |
dc.subject | SIR 20 | en_US |
dc.subject | PRI | en_US |
dc.subject | SNI | en_US |
dc.subject | Wallace Rapid Plastimeter | en_US |
dc.subject | SDGs | en_US |
dc.title | Analisis Kualitas Ketahanan pada Crumb Rubber Mutu Sir 20 dengan Metode Plasticity Retention Index (PRI) di PT. Rubber Hock Lie Sunggal Sumatera Utara | en_US |
dc.title.alternative | Analysis of Durability Quality in Crumb Rubber Quality Sir 20 with Plasticity Retention Index (PRI) Method at PT. Rubber Hock Lie Sunggal North Sumatera | en_US |
dc.type | Thesis | en_US |
dc.identifier.nim | NIM212401027 | |
dc.identifier.nidn | NIDN0028026605 | |
dc.identifier.kodeprodi | KODEPRODI47401#Kimia | |
dc.description.pages | 64 Pages | en_US |
dc.description.type | Kertas Karya Diploma | en_US |